| Crystal growth process: | Mono CVD |
| Size | Length 4 * Width 0.7 * Thickness 0.7 |
| Color | nearly transparent |
| Advantage: | 1) Regular shape, uniform size. The size can be strictly controlled according to customer needs. |
| 2) High repurchase rate and high cost performance, well received by customers. | |
| 3) No visible growth lines, no black spots, no impurities, no crack. | |
| Shape: | Retangular logs |
| Edges | Laser Cut |
| Laser Kerf | < 3° |
| Lateral Tolerance: | +0.1/-0 mm |
| Roughness, Ra | Two sides polished, Ra < 30 nm |
| Thickness Tolerance | +/- 0.05 mm |
| Other available size | 1mm - 15mm |
| Other available thickness | 0.1- 5mm |
| Micro-hardness | 80-150Gpa |
| Young modulus | 1150-1130Gpa |
| Boron Concentration [B]: | <0.05 ppm |
| Nitrogen Concentration: | Mechanical grade 50 ppm - 100 ppm |
MCD Diamond CVD Diamond Polished Diamond Rough Diamond Diamond Abrasive PCD & PDC